Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.057 g/cc | 0.03819 lb/in³ | |
Dow Nordel® IP 4520 Molded Golf Grip FormulationNordel® IP 4520 |
|||
Density | 1.057 g/cc | 0.03819 lb/in³ | |
Dow Nordel® IP 4640 Molded Golf Grips FormulationNordel® IP 4640 |