Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.048 g/cc | 0.03786 lb/in³ | ISO 1183 |
Styrolution Polystyrol 158 K GR 2 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | ISO 1183 |
Styrolution Polystyrol 158 K GR 21 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | ISO 1183 |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | ISO 1183 |
Styrolution Polystyrol 168 N GR 21 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | ISO 1183 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | ISO 1183 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | |
BASF Pluronic® 17 R4 Block Copolymer Surfactant Description: Pluronic 17R4 is a difunctional block copolymer surfactant with terminal secondary hydroxyl groups. A nonionic surfactant that is 100% active and relatively non-toxic.Information provi.. |
|||
Density | 1.048 g/cc | 0.03786 lb/in³ | |
Solvay ANTAROX® 17-R-4 Surfactant Chemical Name: EO/PO BLOCK COPOLYMERCAS: 9003-11-6, 7732-18-5Water solubility: SolubleAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX 17-R-4 is dispersible i.. |