Physical Properties Metric English Comments
Density 0.9826 g/cc
0.03550 lb/in³
Lord Adhesives Chemlok® 610 Adhesive
Chemlok® 610 is an aqueous adhesive used to bond fluoroelastomers, polyacrylates, ethylene acrylic and peroxide vulcanizing EPDM elastomers. Chemlok 610 aqueous adhesive can also be used as a coa..
Density 0.9826 - 1.0065 g/cc
0.03550 - 0.036362 lb/in³
Lord Adhesives Flocklok® 852 Flock Adhesive
LORD Flocklok® 852 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res..