Density | 0.9826 - 1.0065 g/cc | 0.03550 - 0.036362 lb/in³ | |
Lord Adhesives Flocklok® 852 Flock Adhesive LORD Flocklok® 852 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res.. |