Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.981 g/cc | 0.0354 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1001 XV is a C4 Ziegler Natta LLDPE for power cable and Telecom jacketing. The grade contains a low level of antioxidants and has excellent Environmental Stress Crack Resista.. |