Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.8628 - 0.8987 g/cc | 0.03117 - 0.03247 lb/in³ | |
Lord Adhesives Chemlok® 144 Primer LORD Chemlok® 144 primer is a one-coat, moisturecure primer used to prime and/or bond a variety of polar substrates. These substrates include steel, aluminum, brass, e-coated metal, glass fabric,.. |