Lord Adhesives Chemlok® 144 Primer

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Chemlok®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Chemlok® 144 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LORD Chemlok® 144 primer is a one-coat, moisturecure primer used to prime and/or bond a variety of polar substrates. These substrates include steel, aluminum, brass, e-coated metal, glass fabric, architectural and automotive glass, ceramic tile, vitrified clay pipe, concrete and some plastics.Chemlok 144 primer contains a special fluorescent agent used to identify its presence on the material surface when exposed to an ultraviolet (UV) light source. Under normal light, the primer is transparent on the substrate.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.8628 - 0.8987 g/cc
0.03117 - 0.03247 lb/in³
Solids Content 4.8 - 6.2 %
4.8 - 6.2 %
Kinematic Viscosity 1.0 - 8.0 cSt
1.0 - 8.0 cSt
Thermal Properties Metric English Comments
Flash Point 1.70 °C
35.1 °F
Seta
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 88.0 °C
0.0500 hour

@Temperature 190 °F
Shelf Life 12.0 Month

@Temperature 21.0 - 27.0 °C
12.0 Month

@Temperature 69.8 - 80.6 °F
Descriptive Properties Value Comments
Appearance Clear, Light Straw Liquid
Solvents Toluene, n-Butanol, Ethanol