Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.849 g/cc @Temperature 15.6 °C |
0.0307 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn Elite™ 150 Metallocene Polyalphaolefin (mPAO) Fluid Product Description: SpectraSyn ™ metallocene Polyalphaolefin (mPAO) basestock is an advanced high viscosity (Hi-Vis) Polyalphaolefin (PAO). SpectraSyn ™ mPAO utilized metallocene catalyst technol.. |
|||
Density | 0.849 - 0.913 g/cc | 0.0307 - 0.0330 lb/in³ | |
CMT Materials HYTAC® WF High Strength High Clarity 450°F Epoxy Syntactic HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers su.. |
|||
Density | 0.849 g/cc | 0.0307 lb/in³ | |
BNZ Materials 2653LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |