Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.786 g/cc @Temperature 20.0 °C |
0.0284 lb/in³ @Temperature 68.0 °F |
ASTM D4052 |
ExxonMobil IPA Isopropyl Alcohol Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.786 g/cc @Temperature 15.6 °C |
0.0284 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Isopar™ M (AM) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Asia Pacific, Central Ameri.. |
|||
Density | 0.786 g/cc @Temperature 15.0 °C |
0.0284 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Varsol™ 40 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |