Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.785 g/cc | 0.0284 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging JGR-154A Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.785 g/cc | 0.0284 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Density | 0.785 g/cc | 0.0284 lb/in³ | ASTM D1505 |
PolyOne Geon™ Vinyl Packaging XPL189 Amber 1505 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Density | 0.785 g/cc | 0.0284 lb/in³ | |
Pyrotek KF-40 Fiberglass Rope A dense rope with solid fiberglass core covered with a tightly woven Kevlar® jacket. Very abrasion resistant and does not expel fibers quickly.AdvantagesExcellent Abrasion Resistance Excellent Com.. |
|||
Density | 0.786 g/cc @Temperature 20.0 °C |
0.0284 lb/in³ @Temperature 68.0 °F |
ASTM D4052 |
ExxonMobil IPA Isopropyl Alcohol Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.786 g/cc @Temperature 15.6 °C |
0.0284 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Isopar™ M (AM) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Asia Pacific, Central Ameri.. |
|||
Density | 0.786 g/cc @Temperature 15.0 °C |
0.0284 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Varsol™ 40 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |
|||
Density | 0.785 - 0.817 g/cc | 0.0284 - 0.0295 lb/in³ | |
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic HYTAC-FLXT is a unique material, combining the toughness and higher friction of FLX with improved release characteristic through PTFE impregnation. The result is a new, tough syntactic with just th.. |
|||
Density | 0.785 g/cc | 0.0284 lb/in³ | ASTM C134 |
BNZ Materials PA 26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |