Physical Properties Metric English Comments
Density 0.705 g/cc
0.0255 lb/in³
Dry
Unifrax Fibermax® Duraboard® 17H Board
Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. ..
Density 0.705 g/cc
0.0255 lb/in³
Dry
Unifrax Fibermax® Duraboard® 18H Board
Duraboard® 1700 and Duraboard® 1800 are an extension to the Fibermax® product line. These board products exhibit excellent thermal stability (low shrinkage) at very high operating temperatures. ..
Density <= 0.705 g/cc
<= 0.0255 lb/in³
Engineered Syntactic Systems PSF-42 Polyester Subsea Syntactic Void Filler
PSF-42 was developed by Navy subcontractors for simple shipyard-based cavity pours of Naval vessels. This system may be used in any free-flood cavity or void, but is especially valuable in difficult..
Density 0.705 - 0.716 g/cc
0.0255 - 0.0259 lb/in³
ASTM D4052
ExxonMobil Heptene
Appearance: Clear, free of suspended matterInformation provided by ExxonMobil
Density 0.705 g/cc
0.0255 lb/in³
CMT Materials CTB 44 Composite Toolboard High Temperature
CTB-44 is manufactured by CMT Materials for a wide variety of vacuum forming applications. It is suitable for use up to 2500F (1210C). CTB-44 utilizes a copolymer base material and smaller cell st..
Density 0.705 g/cc
0.0255 lb/in³
CMT Materials HYTAC® C Castable Syntactic Tooling
HYTAC-C is a one-part castable product in the HYTAC family of syntactics. This product is available as an uncured, single component mixture that may be poured or cast into a wide variety of shapes a..
Density 0.705 - 0.769 g/cc
0.0255 - 0.0278 lb/in³
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic
HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. ..
Density 0.705 g/cc
0.0255 lb/in³
ASTM C134
BNZ Materials PA 23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Density 0.705 g/cc
0.0255 lb/in³
ASTM C134
BNZ Materials Zelieblok 2000S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.