Polymer Property : Density = 0.620 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.620 - 0.620 g/cc

@Temperature 50.0 - 50.0 °C
0.0224 - 0.0224 lb/in³

@Temperature 122 - 122 °F
Average value: 0.620 g/cc Grade Count:1
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Density 0.620 g/cc
0.0224 lb/in³
Sharadaa Ceramics Vacuum Formed Boards
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Density 0.620 g/cc
0.0224 lb/in³
Foam
Aptek DI-STRATE 95217 Microwave/RF Foam Substrate
DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Information provided by Aptek Laboratories, Inc.