Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.620 - 0.620 g/cc @Temperature 50.0 - 50.0 °C |
0.0224 - 0.0224 lb/in³ @Temperature 122 - 122 °F |
Average value: 0.620 g/cc Grade Count:1 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Density | 0.620 g/cc | 0.0224 lb/in³ | |
Sharadaa Ceramics Vacuum Formed Boards Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.620 g/cc | 0.0224 lb/in³ | Foam |
Aptek DI-STRATE 95217 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Information provided by Aptek Laboratories, Inc. |