Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 13.38 g/cc | 0.4834 lb/in³ | |
Wall Colmonoy COLMONOY® 705 - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide Description and Application: A tough nickel-chromium-boron matrix alloy holds extremely hard tungsten-carbide particles used for protection from severe sliding abrasion. Used on screw conveyors and.. |