Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wall Colmonoy COLMONOY® 705 - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide

Category Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy , Tungsten Alloy
Manufacturer Wall Colmonoy Corporation
Trade Name COLMONOY®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wall Colmonoy COLMONOY® 705 - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description and Application: A tough nickel-chromium-boron matrix alloy holds extremely hard tungsten-carbide particles used for protection from severe sliding abrasion. Used on screw conveyors and augers. Finished by grinding.Method of Application: Fusewelder Information provided by Wall Colmonoy Corporation.
Physical Properties Metric English Comments
Density 13.38 g/cc
0.4834 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 58 - 63
58 - 63
Component Elements Properties Metric English Comments
Boron, B 1.5 %
1.5 %
Carbon, C 2.2 %
2.2 %
Chromium, Cr 7.0 %
7.0 %
Cobalt, Co 0.10 %
0.10 %
Iron, Fe 2.0 %
2.0 %
Nickel, Ni 37.1 %
37.1 %
As Balance
Silicon, Si 1.9 %
1.9 %
Tungsten, W 48.2 %
48.2 %
Processing Properties Metric English Comments
Processing Temperature 1024 °C
1875 °F
fusing temperature