Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.192 - 0.384 g/cc | 0.00694 - 0.0139 lb/in³ | |
Pyrotek M-13 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Non-conductive insulation Lid gaskets AdvantagesDurable Resistant to chemical attack Excellent mechanical strength Low air permeability Information provided by P.. |