Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.192 - 0.384 g/cc | 0.00694 - 0.0139 lb/in³ | |
Pyrotek M-13 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Non-conductive insulation Lid gaskets AdvantagesDurable Resistant to chemical attack Excellent mechanical strength Low air permeability Information provided by P.. |
|||
Density | 0.161 - 0.385 g/cc | 0.00582 - 0.0139 lb/in³ | Typical production range 5 - 12% relative density |
ERG Aerospace Duocel® Silicon Carbide Foam Silicon Carbide (SiC) foam is a porous, open-celled structure made from an interconnected lattice of ceramic ligaments. The pattern of cells and ligaments repeats regularly throughout the entirety o.. |