Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.54 g/cc | 0.309 lb/in³ | |
Indium Corp. Indalloy® 174 Bi-In-Sn Fusible Alloy Environmentally safe fusible alloy. Contains no lead or cadmium.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 8.56 g/cc | 0.309 lb/in³ | |
Indium Corp. Indalloy® 281 Bi-Sn Solder Alloy Good low melting point solder for electronics assembly of for applications where Cd and Pb are to be avoided, and for thermo-electric applications. Shear rate sensitive.Information provided by the m.. |
|||
Density | 8.55 g/cc | 0.309 lb/in³ | |
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |
|||
Density | 8.54 g/cc | 0.309 lb/in³ | |
Special Metals NIMONIC® Alloy 86 A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°.. |
|||
Density | 8.56 g/cc | 0.309 lb/in³ | |
AIM 58Bi/42Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |