Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.2994 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 8.287 g/cc
0.2994 lb/in³
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
Density 8.287 g/cc
0.2994 lb/in³
Carpenter BioDur™ CCM® Medical Implant Alloy, Warm Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
Density 8.287 g/cc
0.2994 lb/in³
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked
Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur Carpenter CCM alloy..
Copyright © lookpolymers.com All Rights Reserved