Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.35 g/cc | 0.229 lb/in³ | |
Indium Corp. Indalloy® 60 Ga-In Eutectic Alloy for Mercury Replacement Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 6.35 g/cc | 0.229 lb/in³ | Sintered |
Ametek P316L P/M Stainless Steel, Sintered from 6.25 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |
|||
Density | 6.33 g/cc | 0.229 lb/in³ | |
Ametek P303L P/M Stainless Steel, Sintered from 6.23 g/cc Green Density Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearate. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Density | 6.35 g/cc | 0.229 lb/in³ | |
Ferro CF 7572 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |