Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.13 g/cc | 0.221 lb/in³ | Sintered |
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.00 g/cc Green Density P409L/409CB is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance .. |
|||
Density | 6.13 g/cc | 0.221 lb/in³ | |
Ametek P410L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for .. |
|||
Density | 6.12 g/cc | 0.221 lb/in³ | |
ATI Wah Chang Vanadium Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores.. |
|||
Density | 6.13 g/cc | 0.221 lb/in³ | Sintered |
Ametek P409L P/M Stainless Steel, Sintered from 6.00 g/cc Green Density P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and ha.. |
|||
Density | 6.12 g/cc | 0.221 lb/in³ | |
Ametek Ultra 303L P/M Stainless Steel, Sintered from 6.0 g/cc Green Density Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i.. |