Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.194 g/cc | 0.00700 lb/in³ | |
Saint-Gobain COHRlastic® F-12 Silicone Foam Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, constr.. |