Physical Properties Metric English Comments
Density 0.194 g/cc
0.00700 lb/in³
Saint-Gobain COHRlastic® F-12 Silicone Foam
Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, constr..