Density 0.186 g/cc
0.00671 lb/in³
Unifrax Excelfrax® 200 VIP Vacuum Insulation Panel
Excelfrax® 200 VIP is a Vaccum Insulation Panel (VIP) designed to provide insulation at temperatures between -300°F and +300°F. This thermal insulation provides extremely low thermal conductivit..