Polymer Property : Density = 0.185 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 5.12 g/cc
0.185 lb/in³
ISO 1183
Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 5.12 g/cc
0.185 lb/in³
MarkeTech Strontium Titanate (SrTiO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.