Physical Properties Metric English Comments
Density 4.48 g/cc
0.162 lb/in³
Kobe Steel KS3-2.5 Alpha-Beta Titanium Alloy, ASTM Gr. 9, Annealed
Nominal Composition: Ti-3 Al-2.5 V Applications: Exhaust systems, bicycle frames, eye glass frames.Features:High strength, excellent balance between strength and toughness.Information provided by K..
Density 4.48 g/cc
0.162 lb/in³
Haynes Ti-3Al-2.5V Alloy Titanium Tubing
Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani..
Density 4.49 g/cc
0.162 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6
LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity.
Density 4.49 g/cc
0.162 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Density 4.49 g/cc
0.162 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific)
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Annealed Bar 0.5 - 1.23 in. dia
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Solution Treated Annealed Bar 0.5 - 1.23 in. dia
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded, Mill Annealed
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.48 g/cc
0.162 lb/in³
ATI Allvac® 3-2.5 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems.
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Density 4.49 g/cc
0.162 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific)
LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Density 4.48 g/cc
0.162 lb/in³
ATI Wah Chang TI-3Al-2.5V
Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working an..