Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | <= 0.146 g/cc | <= 0.00527 lb/in³ | |
ACC EP AOSR EPI Engineered Polymers Acrylic Oligomer EP AOSR, is an aliphatic triacrylate oligomer and is "Powered by Reactamine ®Technology”. EP AOSR is light in color and has fast cure response to UV and EB. EP AOSR exhibits good flexibility, toug.. |