ACC EP AOSR EPI Engineered Polymers Acrylic Oligomer

Category Polymer , Thermoset
Manufacturer Amber Chemical Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC EP AOSR EPI Engineered Polymers Acrylic Oligomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EP AOSR, is an aliphatic triacrylate oligomer and is "Powered by Reactamine ®Technology”. EP AOSR is light in color and has fast cure response to UV and EB. EP AOSR exhibits good flexibility, toughness, abrasion resistance, water resistance, and excellent non-yellowing properties. EP AOSR when used in unsaturated polyesters, allows the styrene monomer content to be reduced to lower V.O.C.’s. Impact strength in gel coats improves, UV stability improves, water resistance increases, and gloss retention is higher. Laminating resin improve in cure and Barcol hardness.Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Density <= 0.146 g/cc
<= 0.00527 lb/in³
Solids Content 100 %
100 %
Polymer Solid
Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
Molecular Weight 1500 g/mol
1500 g/mol
Optical Properties Metric English Comments
Gardner Color Number <= 1.0
<= 1.0