Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.82 - 3.90 g/cc | 0.138 - 0.141 lb/in³ | Sintered Density |
Nabaltec GRANALOX® NM 9923 Ceramic Bodies Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum .. |
|||
Density | 3.81 g/cc | 0.138 lb/in³ | |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Density | 3.81 g/cc | 0.138 lb/in³ | |
Ferro IX 2683 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and ca.. |
|||
Density | 3.83 g/cc | 0.138 lb/in³ | DIN EN 623-2 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Density | 3.81 g/cc | 0.138 lb/in³ | ASTM-C 20 |
CoorsTek ADD-96 96% Alumina |
|||
Density | 3.82 g/cc | 0.138 lb/in³ | ASTM C20 |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Density | 3.82 g/cc | 0.138 lb/in³ | DIN EN 623-2 |
CeramTec B 40 Alumina, 99.1% B 40 is the ideal sliding mate with the same properties as Rubalit® A 1896. It contains a larger share of Al2O3 for superior chemical stability. |
|||
Density | 3.82 g/cc | 0.138 lb/in³ | |
CeramTec Rubalit® A 1896 brown Alumina CeramTec AG's seal and regulator discs are made mainly of Rubalit® A 1896, a material developed especially for this application that is noted for the following special properties: outstanding hard.. |