Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.25 g/cc | 0.117 lb/in³ | ISO 1183 |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Density | 3.25 g/cc | 0.117 lb/in³ | ISO 1183 |
LATI LATAMID 12 H FE90 Nylon 12 Base Magnetizable Compound
(Unverified Data**) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Density | >= 3.25 g/cc | >= 0.117 lb/in³ | |
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ.. |
|||
Density | >= 3.25 g/cc | >= 0.117 lb/in³ | |
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ.. |
|||
Density | 3.25 - 3.35 g/cc | 0.117 - 0.121 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel PTFE G Special Compound with steelInformation provided by Guarniflon® |
|||
Density | 3.23 g/cc | 0.117 lb/in³ | |
LATI Latamid 12 CP/85 PA 12 Polyamide 12 (PA12) based compound. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Density | 3.25 g/cc | 0.117 lb/in³ | |
Ferro EG 2927 Metal Sealing Glass Type: Sr-B-Al Typical Powder Form: VSD Typical Application: Comp. - Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched .. |
|||
Density | 3.25 g/cc | 0.117 lb/in³ | Apparent |
Gouda Vuurvast AK 99 Dense Refractory Brick Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T.. |
|||
Density | 3.23 g/cc | 0.117 lb/in³ | |
Schott BG34 Conversion Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include FG3, FG13 |
|||
Density | 3.25 g/cc | 0.117 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0325 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityTPC# 6066102Information provided by TP Composites, Inc. |
|||
Density | 3.25 g/cc | 0.117 lb/in³ | DIN EN 623-2 |
CeramTec SL 303 Silicon Nitride, SiAION+SiC SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i.. |
|||
Density | 3.24 g/cc | 0.117 lb/in³ | |
Tokuyama Shapal™ SH-50 Sintered Aluminum Nitride Uniform, large sized pressed sintered aluminum nitride. |
|||
Density | >= 3.24 g/cc | >= 0.117 lb/in³ | |
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4) EKatherm® Silicon Nitride is the state-of-the-art material for a wide variety of components used in Aluminum Alloy casting processes.Features: High Temperature Resistance High Thermal Shock Resist.. |