Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.66 - 2.94 g/cc | 0.0961 - 0.106 lb/in³ | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Density | 2.66 - 2.94 g/cc | 0.0961 - 0.106 lb/in³ | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |