Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.624 g/cc | 0.09480 lb/in³ | |
AGY ADVANTEX® Generic Glass Fiber OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.Information provided by AGY Holding Corp... |