Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.32 g/cc | 0.0838 lb/in³ | ISO 1183-1 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Density | 2.32 g/cc @Temperature 25.0 °C |
0.0838 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8271 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization. Used for sealing glass to KOVAR metal and backlights. The heavy metal content for the elements lead, cadmium, mercury, and hex.. |
|||
Density | 2.32 g/cc | 0.0838 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0232 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.32 g/cc | 0.0838 lb/in³ | |
Zircar Refractory Composites RS-DM Refractory Sheet TYPE RS-DM Sheet is a moldable form of Type RS-D with a higher density than obtainable from Refractory Sheet Type RS-DA. Type RS-DM is ideally suited for fabricating complex shapes from a flat sheet.. |
|||
Density | 2.32 g/cc | 0.0838 lb/in³ | |
COI Ceramics Nicalon™ HRV SiCO Ceramic Fiber Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties .. |