Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0600 - 0.0760 g/cc | 0.00217 - 0.00275 lb/in³ | sheet density |
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0640 - 0.0760 g/cc | 0.00231 - 0.00275 lb/in³ | |
Akzo Nobel Expancel® 461 DE 20 d70 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |