Polymer Property : Density = 0.00231 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0640 g/cc
0.00231 lb/in³
Pyrotek L-4 Fiberseal Blanket
Lightweight, yet strong and durable needled blankets.Dimensions610 mm x 7.6 m1219 mm x 7.6 m6 - 51 mm thickApplicationsFurnace linings Gaskets Expansion joints Fire blanket Fire pillowsInformation p..
Density 0.0640 g/cc
0.00231 lb/in³
Pyrotek M-2 Fiber Seal Pre-cut Gasket
A light-brown ceramic fiber material. Excellent trough gasket material.Information provided by Pyrotek.
Density 0.0640 g/cc
0.00231 lb/in³
Pyrotek M-2 High-Temperature Felt
A light-brown material.Dimensions457 mm x 7.6 m 25 mm thickApplicationsHigh-temperature gasketsInformation provided by Pyrotek.
Density 0.0641 - 0.128 g/cc
0.00231 - 0.00463 lb/in³
Monmouth Rubber & Plastics Durafoamâ„¢ DK1111 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.0641 - 0.128 g/cc
0.00231 - 0.00463 lb/in³
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend
Information provided by Monmouth Rubber & Plastics Corp.
Density 0.0641 g/cc
0.00231 lb/in³
Available
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator
Fiberfrax Durablanket HP-S insulation is a needled blanket made from spun Fiberfrax ceramic fibers. Durablanket HP-S insulation combines all of the physical characteristics offered by Durablanket S..
Density 0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Density 0.0640 - 0.128 g/cc
0.00231 - 0.00462 lb/in³
Thermal Ceramics Cerachem Blanket Strip
Thermal Ceramics Kaowool® Strip products are cut from either Kaowool Blanket, Blanket S, Cerablanket®, or Cerachem® Blanket. These products are available in many forms and lengths depending upon ..
Density 0.0640 - 0.128 g/cc
0.00231 - 0.00462 lb/in³
Thermal Ceramics Cerachem Mesh Enclosed Rounds, Strips and Blankets
Kaowool ceramic fiber blankets can be encased in stainless steel wire meshes for many useful purposes. The wire mesh alloy used is determined by the atmosphere and temperature the enclosed product w..
Density 0.0640 g/cc
0.00231 lb/in³
Thermal Ceramics Micro-Foil Type 475 Insulating Tape
Features: Easy to use Flexible Variety of thicknesses and sizesApplications Fuel, oil and hydraulic lines Ducts Compressors and de-icing equipment High temperature tubing and piping systems A variet..
Density 0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
Thermal Ceramics Superwool 607 Blanket
Superwool is designed from pure raw materials and specially processed to offer excellent performance in high temperature applications. Superwool offers an alternative to traditional solutions due to..
Density 0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
Thermal Ceramics Superwool 607 Max Blanket
Superwool is designed from pure raw materials and specially processed to offer excellent performance in high temperature applications. Superwool offers an alternative to traditional solutions due to..
Density 0.0640 - 0.0860 g/cc
0.00231 - 0.00311 lb/in³
sheet density
Zotefoams Plastazote® HL79 Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0641 g/cc
0.00231 lb/in³
Hexcel® HexWeb® HRH-10 - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb® HRH-10 is manufactured from NOMEX® aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to t..
Density 0.0641 g/cc
0.00231 lb/in³
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Density 0.0641 g/cc
0.00231 lb/in³
Hexcel® HexWeb® HRH-327 - 3/8 - 4.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Density 0.0641 g/cc
0.00231 lb/in³
Hexcel® HexWeb® HRP - 3/16 - 4.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This pr..
Density 0.0641 g/cc
0.00231 lb/in³
Unifrax Fiberfrax® Duraback® Ceramic Fiber Insulator
Fiberfrax Duraback blanket is a strong, lightweight, flexible needled blanket intended for use as a cost-effective back-up insulation in Fiberwall® furnace linings. It is recommended for use up to..
Density 0.0641 g/cc
0.00231 lb/in³
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb® HRH-10 is manufactured from NOMEX® aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to t..
Density 0.0640 g/cc
0.00231 lb/in³
Molded density, ASTM D1622
Covestro Bayfill® EA 2003 Polyurethane Energy-Absorbing Semi-Rigid Foam, Friable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 0.0640 g/cc
0.00231 lb/in³
Molded density, ASTM D1622
Covestro Bayfill® EA 6004 Polyurethane Energy-Absorbing Semi-Rigid Foam, Recoverable Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 0.0640 g/cc
0.00231 lb/in³
ASTM D3574A
Covestro Bayfit® SA Polyurethane Sound Absorbing Foam, High-Resilience, Higher density
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Density 0.0640 g/cc
0.00231 lb/in³
DIN 53420
Dow STRANDFOAM™ EA 1600 Polypropylene Foam
STRANDFOAM™ EA 1600 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra..
Density 0.0640 g/cc
0.00231 lb/in³
3M 4466W Double Coated Polyethylene Foam Tape
3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in..
Density 0.0641 g/cc
0.00231 lb/in³
Monmouth Rubber & Plastics Durafoam™ C19XLDS EPDM
Special Features: Extremely soft and conforms easily to irregular surfaces Superior buoyancy Excellent chemical resistance 100% free of HCFC & CFC Available in custom colors upon request for quoteCo..
Density 0.0640 g/cc
0.00231 lb/in³
Available in multiple densities from manufacturer
Thermal Ceramics Kaowool Blanket
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens..
Density 0.0640 - 0.0760 g/cc
0.00231 - 0.00275 lb/in³
Akzo Nobel Expancel® 461 DE 20 d70 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0641 g/cc
0.00231 lb/in³
Free Rise Density
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..
Density 0.0641 g/cc
0.00231 lb/in³
ASTM D3575
Monmouth Rubber & Plastics Durafoam™ PMR 150 EPDM
Performance Features: Softness, stiffness & density infinitely variable.High Ozone Resistance. High Ultraviolet Resistance. Non-Staining. Made from Heat Resistant EPDM Non-fogging (plasticizer free..
Density 0.0640 g/cc
0.00231 lb/in³
Pyrotek M-4 Fiberseal Blanket
A white high-temperature felt.Dimensions610 mm x 15.2 m25 mm thickApplicationsGaskets Trough covers Trough gaskets Information provided by Pyrotek.