Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.180 - 1.99 g/cc | 0.00650 - 0.0717 lb/in³ | Average value: 1.03 g/cc Grade Count:671 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |