Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.00650 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.180 - 0.250 g/cc
0.00650 - 0.00903 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli..
Density 0.180 g/cc
0.00650 lb/in³
Sharadaa Ceramics Saber Block, Pyroblock
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Density 0.180 - 0.240 g/cc
0.00650 - 0.00867 lb/in³
ISO 1183
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam
EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds
Density 0.180 - 0.220 g/cc
0.00650 - 0.00795 lb/in³
ISO 845-88
Eurofoam Siliconcell 412/BT 130 Silicone Foam
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Density 0.180 - 0.220 g/cc
0.00650 - 0.00795 lb/in³
True, 3M QCM 14.24.6
3M A20/1000 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.180 - 0.220 g/cc
0.00650 - 0.00795 lb/in³
True, 3M QCM 14.24.6
3M H20/1000 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.180 - 0.220 g/cc
0.00650 - 0.00795 lb/in³
3M K20 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.180 - 1.99 g/cc
0.00650 - 0.0717 lb/in³
Average value: 1.03 g/cc Grade Count:671
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Density 0.180 - 0.220 g/cc
0.00650 - 0.00795 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Copyright © lookpolymers.com All Rights Reserved