Polymer Property : Density = 0.06774 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.875 g/cc
0.06774 lb/in³
Pyrotek Pyrocast TG Castable Refractory
Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.ApplicationsCoreless induction furnace lining Channel..