Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.83 g/cc | 0.0662 lb/in³ | Slurry |
Omya OMYAFLOW® 3 - SY Calcium Carbonate A beneficiated calcium carbonate with excellent fineness, color, and dispersion characteristics available in dry and slurry forms.Applications: Decorative paints.Information supplied by Omya North A.. |
|||
Density | 1.83 g/cc | 0.0662 lb/in³ | |
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |