Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 - 1.77 g/cc | 0.0427 - 0.0640 lb/in³ | Average value: 1.66 g/cc Grade Count:7 |
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum.. |