Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Density | 1.38 - 1.77 g/cc | 0.0499 - 0.0639 lb/in³ | Average value: 1.45 g/cc Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v.. |
|||
Density | 1.18 - 1.77 g/cc | 0.0427 - 0.0640 lb/in³ | Average value: 1.66 g/cc Grade Count:7 |
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum.. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF) Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanical.. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF) Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically .. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | Stand relative density |
Shandong Dongyue Shenzhou New Material Co DS201 Polyvinylidene Fluoride Powder Conformable with: Q/DYS 014-2007Polyvinylidene fluoride (PVDF) powder (DS201) PVDF is the homopolymer of vinylidene fluoride, which is excellent chemical corrosion-resistant, high temperature resist.. |
|||
Density | 1.75 - 1.77 g/cc | 0.0632 - 0.0639 lb/in³ | ASTM D1505 |
Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF) Hylar® 301F is a high melt viscosity polyvinylidene fluoride (PVDF) powder used for non-architectural dispersion coatings.Features: High Viscosity; HomopolymerUses: Coating ApplicationsAdditiona.. |
|||
Density | 1.33 - 1.77 g/cc | 0.0480 - 0.0639 lb/in³ | Average value: 1.56 g/cc Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |
|||
Density | 1.05 - 1.77 g/cc | 0.0379 - 0.0639 lb/in³ | Average value: 1.49 g/cc Grade Count:58 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |