Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.7354 g/cc | 0.062691 lb/in³ | |
Saint-Gobain Chemfab® 3 Industrial PTFE-Coated Glass Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, g.. |
|||
Density | 1.7354 g/cc | 0.062691 lb/in³ | |
Saint-Gobain Chemfab® 5 Basic PTFE-Coated Glass Description: Chemfab® Basic Series products are low resin-content, non-porous, PTFE-coated fiberglass fabrics. Applications are spray shields, separator sheets, release sheets and protective barrie.. |