Saint-Gobain Chemfab® 3 Industrial PTFE-Coated Glass

Category Ceramic , Glass , Glass Fiber
Manufacturer Saint-Gobain Quartz PLC
Trade Name Chemfab®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Chemfab® 3 Industrial PTFE-Coated Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Chemfab® Industrial Series products are multi-purpose, non-porous, medium-resin content, PTFE-coated fiberglass fabrics. Applications include release sheets, packaging, composites, gaskets, etc. Chemfab Industrial is a high-value product delivering both price and performance. All data based on a 0.003 inch test sample. Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Density 1.7354 g/cc
0.062691 lb/in³
Mechanical Properties Metric English Comments
Tear Strength Test 2.0
2.0
Lbs./In. Propagation Tear Strength in fill/transverse direction
3.0
3.0
Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 14.0 kN/m
80.0 pli
Tensile Strength (Fill)
14.9 kN/m
85.0 pli
Tensile Strength (Warp)
Descriptive Properties Value Comments
Weight (oz/yd^2) 3.9