Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.68 g/cc | 0.0606 lb/in³ | |
Devcon Brushable Ceramic - Red, Blue Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |
|||
Density | 1.68 g/cc | 0.0606 lb/in³ | |
Devcon Brushable Ceramic - White Epoxy Precision Repair EpoxyComments: Low-viscosity, alumina-filled, brushable epoxy compound, when applied to a 15-20 mil coating, provides a smooth, protective barrier against wear, abrasion, corrosion,.. |