Physical Properties Metric English Comments
Density 1.635 g/cc
0.05907 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific)
LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform..
Density 1.635 g/cc
0.05907 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched
LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.
Density 1.635 g/cc
0.05907 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific)
LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa..