Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.61 g/cc | 0.0581 lb/in³ | |
Devcon Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Density | 1.61 g/cc | 0.0581 lb/in³ | |
Devcon High-Performance Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Density | 1.61 g/cc | 0.0581 lb/in³ | |
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |