Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.536 g/cc | 0.05549 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |