Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.499 g/cc | 0.05415 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® CE15315 NC010 PBT
(Unverified Data**) Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |