Polymer Property : Density = 0.0497 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.14 - 1.38 g/cc
0.0412 - 0.0497 lb/in³
Average value: 1.25 g/cc Grade Count:10
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..