Polymer Property : Density = 0.04473 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.238 g/cc
0.04473 lb/in³
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..